Research Interests            Publications and Patents

 

 

 

 

 

 

 

 

 

 

 

 

 

SEM micrographs illustrating the fibrous structure of the electrospun human, fibrinogen scaffold 

composed of 80 ± 30 nm fiber diameter.

 

 

Photograph of a cotton gauze (left) and an electrospun bovine fibrinogen mat (right) 

produced from 0.167 g/ml fibrinogen in HFP/MEM that is approximately 6 x 6 cm 

with a thickness of 0.7 mm (dry mass is approximately 0.08 grams) for potential use 

as a tissue engineering scaffold or wound dressing.

 

 

Send mail to edboland@vcu.edu with questions or comments about this web site.
Last modified: March 23, 2004